Glass fiber reinforced polyamide 6.6

Polyamide 6.6 30% glass fiber reinforced.
It exhibits high stiffness, toughness, impact resistance, resistance to thermal distortion, has low friction and wear coefficient.
Softening temperature 240ºС.